Comparison Of Microstructure And Texture Development Of Ecaped Pure Mg With A Mg-Si Alloy

Weimin Gan,Heinz Günter Brokmeier,Mingyi Zheng,Hai Chang,Xiaojun Wang,Kun Wu
2008-01-01
Archives of Metallurgy and Materials
Abstract:The evolution of microstructures and texture during ECAP processing of pure Mg and Mg-Si alloy with route A were investigated. The results showed, that the degree of grain size refinement for pure Mg was limited after 2 passes, because of a relatively high processing temperature. Two different types,of Mg-2 Si were obtained: firstly, relatively coarse polygonal Mg-2 Si grains and secondly, the Chinese type eutectic mixture of Mg with Mg2Si. These hard particles Of Mg-2 Si have an high influence on the development of texture and microstructure during ECAP. A kind of basal-plane-type texture was formed for both materials, where the (0002) pole figure showed a strong orientation maximum, normal to the deformation plane. The misfits from the ideal 45 degrees tilting angle related to the 90 degrees die geometry come from the construction details of the ECAP device. The monoclinic deformation symmetry by shearing was not reached because of friction, which resulted in a simple rotation along the ECAP-direction.
What problem does this paper attempt to address?