Manufacture of a new style diamond grinding wheel with Al-based bonding matrix

Shuangxi Wang,Xuejing Liu,Biao Geng,Lin Geng
DOI: https://doi.org/10.19591/j.cnki.cn11-1974/tf.2008.05.006
2008-01-01
Abstract:A new style diamond grinding wheel with Al-based bonding matrix was prepared in this paper. The influence of sintering temperature on the relative density, hardness and working life of diamond grinding wheels with Al-Sn-Ti, Al-Sn-Ti-Ni-Co, Al-Sn-Ti-Ni, Al-Sn-Ni-Co bonding matrix was studied. The microstructure of different bonding matrix sintered at different temperature was observed. The service performance was compared with Cu-based or resin-based grinding wheel. The results show that, Al-Sn-Ti-Ni-Co is the better composition, and the best sintering temperature is 300°C. The samples were compacted after sintered at 300°C; Al-based bonding matrix is strongly retentive of diamond. The working life of this Al-based new type diamond grinding wheel is about two times as long as that of resin-bonded grinding wheel.
What problem does this paper attempt to address?