HIGH TEMPERATURE OXIDATION BEHAVIOR OF Fe40Al/TiC COMPOSITES

Mingxia GAO,Shengcai Zhang,Zhiqiang SHEN,Huage ZHANG,Feng YU,Yi PAN
DOI: https://doi.org/10.3969/j.issn.1005-4537.2007.04.012
2007-01-01
Abstract:TiC matrix Fe40Al intermetallic composites were made by spontaneous infiltration. The oxidation kinetics of Fe40Al/80vol%-88vol%TiC composites were investigated by means of conducting the oxidation experiments in air at temperature of 700 °C - 1100 °C for up to 65 hours, and measuring the variations of the weight gains of the composites with the oxidation times. The microstructure evolution of the composites during the oxidation processing was studied by using SEM/EDS and XRD. The effect of the surface roughness of the composites on the oxidation behavior was also studied. The results show that, the weight gain data were fitted a power type law with the oxidation time with power coefficients ranging 0.63 - 0.75, the oxidation rate decreased with increasing the oxidation time. The oxidation layer was mainly composed of dense crystalline TiO 2, the crystalline size of TiO 2 was effected by the oxidation temperature and the surface roughness of the composiles.
What problem does this paper attempt to address?