Preparation and Microstructure of Nanocrystalline Fe-Ni-Mo Alloy with Low Mo and High Fe Content

LUO Bei-ping,GONG Zhu-qing,REN Bi-ye,YANG Yu-fang,CHEN Meng-jun
DOI: https://doi.org/10.3969/j.issn.1672-7207.2006.04.013
2006-01-01
Abstract:Nanocrystalline Fe-Ni-Mo alloy with low Mo and high Fe content was electrodeposited from acid citrate electrolyte. The surface morphology, microstructure and composition of the alloys were analyzed by scanning electron microscopy, X-ray diffactometry and energy dispersive spectrometry. The results show that the technical parameters and the concentration of sodium molybdate have obvious effect on the composition of the alloy. The crystal grain size is from 6.2 to 12.7 nm and changes with current density, temperature and the pH value of the electrolyte. The crystalline growth of the alloy accords with the model of three-dimensional growth. The surface morphology is mainly determined by the rate competitions between the growing direction of vertical surface and the expanding direction along the surface towards circumambient. The results of the X-ray data show the presence of the multiphase containing solid solution and intermetallic compound in the deposits. The deposit phases alter from the FeNi (BCC) and FeMo solid solution to the FeNi (FCC) and MoNi4 structure at 3 A/dm^2. The deposits internal stress increases linearly with the decrease of the grain size. The lattice parameter of the deposits are slightly distorted because of the residual stress in the deposits.
What problem does this paper attempt to address?