The effects of the parameters of ball milling on the thermal stabilities of the as-milled MgNi amorphous

Mian-wu MENG,Xin-yu LIU,Jun CHENG,Hua-ying ZHOU
DOI: https://doi.org/10.3321/j.issn:1001-9731.2005.05.017
2005-01-01
Abstract:The effects of the parameters of ball milling such as the rate of ball weight, ball to powder weight ratio and the velocity and time of milling on the structural characteristics, thermal stability and phase transformation of the MgNi specimens were investigated by means of X-ray diffraction with high temperature accessory (XRD) and differential thermal analysis (DTA) in this paper. The thermal stabilities of the MgNi amorphous would be reduced with the increasing in the energy of ball milling. When the energy of the as-milled MgNi sample was not high enough (the velocity and time of ball milling was little, ball to powder weight ratio was low, the weight of big balls was higher but the number of small ones was less), the DTA curves of the amorphous specimens consists of only one exothermic peak corresponds to crystallization to Mg2Ni and MgNi2 phases. On the other hand, when the energy of ball milling was high enough, the DTA curves of the samples consists of two exothermic peaks which corresponds to crystallization into Mg2Ni, MgNi2 phases, respectively.
What problem does this paper attempt to address?