Sintering, thermal expansion and mechanical properties of K0.6Sr0.7Zr4P6O24 ceramics

郭兴忠,杨辉,胡晓珍,葛曼珍
DOI: https://doi.org/10.3785/j.issn.1008-973X.2004.07.028
2004-01-01
Abstract:K0.6Sr0.7Zr4P6 O24 (KSZP) ceramics were prepared with KSZP nanometer powder as the raw material synthesized by phosphate direct co-precipitation. The sintering, thermal expansion and mechanical properties of the KSZP ceramics were studied, and the effects of sintering conditions on these properties were analyzed. The obtained suitable sintering conditions for KSZP ceramics are as follows: Nb2O5 additive is 2%, sintering temperature is 1380°C and sintering time is 2 h. The relative density of KSZP ceramics sintered under above conditions is about 94.61% , the bending strength is 91.83 MPa, and the average value of thermal expansion coefficient at 0-600°C is about 1.4×10-6/°C, which is under very low level. The sintering rate is supposed to be rapid, and the crystalline grain does not grow rapidly in the final stage.