Effects of BST Additive on Microstructure and Electromagnetic Parameters of Co2Z-type Hexagonal Ferrite

黄鹏,邓龙江,谢建良,梁迪飞,陈良
DOI: https://doi.org/10.3321/j.issn:1001-9731.2004.02.006
2004-01-01
Abstract:Z-type hexaferrite (Ba_3(Co_(0.4)Zn_(0.6))_2Fe_(23.4)O_(41)) with BST(BaSrTiO_3)additive was prepared by standard ceramic technique. We have investigated the effects of BST additive on sintering temperature, microstructure, grain size and dynamic electromagnetic characteristics in the range of 1MHz~1GHz. The results from XRD and SEM indicate that as the amount of BST increases, the major phase changes to Z-phase, simultaneously M-phase and perovskite phase appear, and the grain size increases. When the weight percent of BST additive in Z-type hexaferrite was varied from 0% to 1.5%, the BST additive not only promoted the sintering density of modified Z-type hexaferrite, but also improved complex permeability and complex permittivity. When BST=1.5wt% and the frequency was 1MHz,μ′=28,e′=100, which was much higher than μ′, e′ of the pure Z-phase hexagonal ferrite. However, ferromagnetic and ferroelectric resonance peaks shift to low frequency region.
What problem does this paper attempt to address?