Preparation of LaGaO_3 Based Electrolyte for Intermediate Temperature SOFC

张乃庆,孙克宁,吴宁宁,周德瑞
DOI: https://doi.org/10.3321/j.issn:1001-9731.2004.04.016
2004-01-01
Abstract:The electrolyte La0.9Sr0.1Ga0.8Mg0.2O3-δ was prepared by the method of solid-state reaction. X-ray diffraction was used to characterize phase transition with the temperature. Test results show that the pure phase is formed by sintering 24 h at 1 500 ℃. The effect of calcine temperature and time were discussed. The powder granularity is 1 μm; and after sintering 15 h at1 500 ℃, the relative density of ceramic can reach 99%. The conductivity was measured by AC impedance. The result was 0.12 S/cm at 800 ℃. The active energy was 0.8 eV at high temperature (≥650 ℃) and 1.09 eV at lower temperature (≤650 ℃) respectively .