Generation and characterization of a protective layer on steel tribosurfaces in presence of Mg6Si4O10(OH)8

He Yang,Zhengye Zhang,Shenghua Li,Yuansheng Jin
2004-01-01
Abstract:A Falex tribotester was employed to in situ generate a protective layer on the 45# steel tribosurfaces under designed tribological conditions in the presence of the magnesium silicate hydroxide (Mg6Si4O10(OH)8) superfine powders, which were finely dispersed in a carrier oil of mineral base. Wear rate of the tribocouple decreased as running time goes on within the initial 50 hr. After an extended operation of 400 hr in total, the formed protective layer grew to ∼ 2 μm in thickness, and mass losses of tribocouple were very little. The surface micro-hardness of the protective layer was twice higher than that of the original un-reconditioned surface, with an average value of Hv780. Initial XPS analysis suggested that the protective layer consist of the oxides and carbides of iron with form of Fe2O3, Fe3O4, and Fe3C. This is an abstract of a paper presented at the 59th STLE Annual Meeting (Toronto, Ontario, Canada 5/17-20/2004).
What problem does this paper attempt to address?