Aging treatment and magnetic properties for the 2: 17 type SmCo permanent magnets of high coercivity

Jianhong Yi,Juan Du,YuanDong Peng,Yali Li,XinWen Tang,ShuDong Luo
DOI: https://doi.org/10.3321/j.issn:1002-185x.2003.10.017
2003-01-01
Rare Metal Materials and Engineering
Abstract:By using X-ray diffraction, scan electron microscope, X-ray electron energy analysis and magnetic measurement, the relationship between magnetic properties and microstructure for the high intrinsic coercivity 2 : 17 SmCo, permanent magnets during aging treatment were investigated. It is found that the alloy decomposed into a 2 : 17 phase and a 1 : 5 phase as soon as the aging treatment started, and the precipitates at grain boundaries have an effect on the enhancement of coercivity. The variation of intrinsic coercivity at different aging processes can be considered as the variation of the domain wall energy difference between the two phases.