Revisiting the pinning sites in 2:17-type Sm-Co-Fe-Cu-Zr permanent magnets

Xianglong Zhou,Yao Liu,Wentao Jia,Xin Song,Andong Xiao,Tao Yuan,Fang Wang,Jiuping Fan,Tianyu Ma
DOI: https://doi.org/10.1016/j.jre.2021.03.013
IF: 4.632
2021-12-01
Journal of Rare Earths
Abstract:Volume fraction of 1:3R platelets can be enlarged by extending the second-step aging time.The abnormally thickened 1:3R platelets interrupt the domain walls, weakening the pinning strength.The 1:5H cell boundaries act as the dominating pinning sites instead of the intersections of 1:3R platelets and cell boundaries.It is still an open debate whether the 1:5H cell boundaries (CBs) or the intersections of 1:3R platelets and 1:5H CBs are the strong pining sites for the cellular nanostructured 2:17-type Sm-Co-Fe-Cu-Zr high temperature permanent magnets despite that they have been widely applied in advanced industries since 1970s. Herein, through tuning the volume fraction of Zr-enriched 1:3R platelets by varying the second-step aging time, the pinning behavior in a model magnet Sm<sub>25</sub>Co<sub>44.9</sub>Fe<sub>21.5</sub>Cu<sub>5.6</sub>Zr<sub>3.0</sub> (wt%) was investigated. The results show that the volume fraction of 1:3R platelets can be effectively enlarged without changing the cell size (i.e. the volume fraction of CBs) by extending the aging time at 400 °C. Combined microscopic TEM characterizations and macroscopic magnetic measurements reveal that the locally thickened 1:3R platelets after long-term second-step aging reduce the effective pinning area by interrupting the magnetic domain walls at CBs, weakening the average pinning strength and the coercivity of the magnet. Consequently, our work supports that the 1:5H CBs act as the dominating pinning sites instead of the intersections of 1:3R platelets and 1:5H CBs, which may provide an important insight towards understanding the hard magnetism of pinning-controlled permanent magnets.The deteriorated coercivity induced by long-term second-step aging (a) is due to the enlarged volume fraction of Zr-enriched 1:3R platelets in grain interiors and (<em>n</em>+1):(5<em>n</em>–1) platelets at grain edges (b, c), which weaken the pinning strength by interrupting the domain walls (d, e).<span class="display"><span><ol class="links-for-figure"><li><a class="anchor download-link u-font-sans" href="https://ars.els-cdn.com/content/image/1-s2.0-S1002072121000648-ga1_lrg.jpg"><span class="anchor-text">Download : <span class="download-link-title">Download high-res image (326KB)</span></span></a></li><li><a class="anchor download-link u-font-sans" href="https://ars.els-cdn.com/content/image/1-s2.0-S1002072121000648-ga1.jpg"><span class="anchor-text">Download : <span class="download-link-title">Download full-size image</span></span></a></li></ol></span></span>
chemistry, applied
What problem does this paper attempt to address?