Primary Observation by Measuring Magnetic Resonance Artifacts Caused by Metallic Dental Materials

Chun Xie,Li-ying YU,Yi ZHOU,Jiang LIN
DOI: https://doi.org/10.3969/j.issn.1672-8467.2001.02.011
2001-01-01
Abstract:Purpose To evaluate the existence and extent of magnetic resonance(MR) artifacts caused by frequently used metallic dental materials and to compare the influence of different MRI sequences on artifacts. Methods A total of 22 kinds and 25 metallic dental samples were tested with 1.5 T MR imager and gradient-echo sequence. Spin-echo and fast spin-echo were added to parts of these samples. Results Of all the 25 metallic dental samples, 11 including gold, amalgam, and silver point did not produce artifact. Titanium alloy and porcelain product fused in metal had mild artifacts. Whereas the remaining 12 samples such as the retention pin and pivot pin showed severe artifacts. Artifacts produced by retention pin, nickel chromium crown and so on were less severe on fast spin-echo. Conclusions Attention should be paid to some of the metallic dental materials, which could cause severe MR artifacts and image degradation, when undergoing face,jaw and head MR examination. Artifacts can be alleviated by using proper metallic materials or choosing proper imaging sequence and parameters.
What problem does this paper attempt to address?