Comparison of MRI artifacts caused by Ni-Cr alloy fixed prostheses on different field-strength magnets

SHAO Chen-ying,YU Li-ying,XIE Chun,LIN Jiang
DOI: https://doi.org/10.3969/j.issn.1674-8115.2008.11.005
2008-01-01
Abstract:Objective To evaluate the influence of different field-strength magnets(1.5 T and 3.0 T)on MRI artifacts caused by Ni-Cr alloy fixed prostheses.Methods The crown,bridge and upper denture fixed prostheses with different thickness were produced by Ni-Cr alloy as test samples,and were one by one put on the centre of water phantom for MR scanning with different field-strength magnets(1.5 T and 3.0 T).The artifact areas on these two field-strength magnets were measured and statistically compared.The plastic prostheses with the same shape and thickness as the test samples were served as controls.Results Ni-Cr alloy fixed prostheses could cause MRI artifacts,and the artifact areas increased with the mass of prostheses.However,no artifact area was found in controls.Compared with those on 1.5 T magnet,the MRI artifact areas significantly increased on 3.0 T magnet(P<0.05).Under the same field-strength,the artifact areas significantly increased by scanning sequence T_1WI than those by T_2WI(P<0.05).Conclusion The lower field strength and fast spin echo sequence should be selected for MRI examinations in patients wearing fixed prostheses made of Ni-Cr alloy.Ni-Cr alloy should be avoided for the fixed prostheses of big mass.
What problem does this paper attempt to address?