Preparation and characterization of nickel-iron hydrotalcites and their derived mixed oxides

Mai Tu,Jianyi Shen,Gufeng Wang,Yi Chen
1997-01-01
Chinese journal of inorganic chemistry
Abstract:A series of NiFe hydrotalcites with Ni/Fe molar ratios of 1,2,3,6 and 10 was synthesized by coprecipitation. TG-DTA results showed that the decomposition of the hydrotalcite samples proceeded in two stages, corresponding to the two endothermic peaks around 200��C and 300��C , respectively. After calcination at 400��C, the hydrotalcites were transformed into NiFeO mixed oxides with high surface areas around 200 m2/g. The mixed oxides thus formed exhibited the same XRD patterns as that of NiO. The mixed oxides still possess the surface area of about 15 m2/g even after calcination at 800��C , higher than that of NiFeO synthesized by the conventional method of coprecipitation. XRD and Moessbauer spectroscopy revealed that Fe3+ cations highly distributed in the lattice of the mixed oxides. In. situ M?essbauer spectroscopy showed that the mixed oxides can be reduced to NiFe alloy at 300��C in H2.
What problem does this paper attempt to address?