Effects of Si addition on properties of Fe-Cr-W-Ti-Y2O3 alloy fabricated by mechanical alloying

Zhenhua Yao,Weihao Xiong,Guopeng Zhang,Xiao Chen,Bin Huang
DOI: https://doi.org/10.1016/j.matdes.2013.11.076
IF: 9.417
2014-01-01
Materials & Design
Abstract:Effects of Si element on characteristics of Fe-Cr-W-Ti-Y2O3 alloy, including relative density, tensile strength, oxidation resistance and microstructure had been investigated. The results showed that the alloy with Si addition appeared superior properties than alloy without Si. The relative density and tensile strength of alloy without Si were only around 85% and 300 MPa, while that of alloy adding Si could reach up to 96.8% and 692.7 MPa after sintering at 1350 degrees C. Mass gain of alloy adding Si was approximately one tenth that of alloy without Si when oxidized at 650 degrees C and 850 degrees C. These superior properties were attributed to action of Si in sintering and oxidation processes. It would activate the sintering for more dense alloy, and form protective oxidized film preventing diffusion of oxygen and metal atoms. (C) 2013 Elsevier Ltd. All rights reserved.
What problem does this paper attempt to address?