SYNTHESIS AND CHARACTERIZATION OF POLYESTERAMIDES DERIVED FROM Ε-Caprolactam AND AMINOETHANOL

Liu Shiyue,Li Chenguo,Zhao Jingbo,Jiang Shengling,Yang Wantai
DOI: https://doi.org/10.3724/sp.j.1105.2012.11041
2012-01-01
Acta Polymerica Sinica
Abstract:Provided a method to synthesize Nylon-6 oligomers with certain molecular weight and to further synthesize polyesteramides having short Nylon-6 segments connected by ester linkages. Polyamide prepolymer (PrePA) with molecular weight of 524. 6 to 808. 1 was synthesized by a ring-opening polymerization of epsilon-caprolactam in the presence of aminoethanol under the catalysis of H3PO3. The chain extension of the PrePAs was studied using N, N'-carbonylbiscaprolactamat (CBC) and 2, 2'-(1, 4-phenylene)-bis (2-oxazoline) (PBOX) as combined chain extenders. Through polycondensation of PrePA with adipic acid, polyesteramide prepolymers(PrePEA) with intrinsic viscosity of 0. 22 similar to 0. 30 dL/g were synthesized. Chain extension of the PrePEAs was carried out using PBOX and CBC as combined chain extenders and the chain extended polyesteramide (ExtPEA) with intrinsic viscosity up to 0. 74 dL/g was obtained. The ExtPEAs were characterized by FTIR and H-1-NMR spectra, differential scanning calorimetry (DSC), thermogravimetric analysis (TGA), wide angle X-ray scattering (WAXS) and tensile test. The DSC study showed that after chain extension the T-m and Delta H-m of the polyesteramides decreased. ExtPEA with [eta] of 0. 72 dL/g had the T-g of 30 degrees C and T-m of 163 degrees C. WAXS characterization showed that the ExtPEA had similar crystal characteristics to the Nylon-6 crystallites. TGA study showed that the ExtPEA had good thermal stability with initial decomposition temperature over 330 degrees C. Tensile test showed that typical ExtPEA samples had a tensile strength of 14. 1 MPa and a strain at break of 68. 6%. The ExtPEA has high Tm, good thermal stability and moderate tensile strength, and is suitable for melt processing. Meanwhile, presence of the ester linkages and lower crystallinity in the ExtPEA may lead to improved biodegradability of the ExtPEA compared to the normal nylon-6.
What problem does this paper attempt to address?