Synthesis of Polyesteramides from N,N '-Bis(2-hydroxyethyl)terephthalamide and Chain Extension Reaction

Huang Chaoqun,Xu Shaoyi,Zhao Jingbo,Jiang Shengling,Yang Wantai
DOI: https://doi.org/10.3724/sp.j.1105.2010.00237
2010-01-01
Acta Polymerica Sinica
Abstract:Polyesteramide(PEA(x/y)) prepolymers with intrinsic viscosity from 0.24 dL/g to 0.52 dL/g were synthesized through melt condensation polymerization from adipic acid,butanediol and N,N′-bis(2-hydroxyethyl)terephthalamide(HETA) at different butanediol(x) to HETA(y) molar ratios.Chain extension reaction was performed with(2,2′-(1,4-phenylene)-bis(2-oxazoline))(PBOX) or adipoyl biscaprolactamate(ABC) alone,or with combined PBOX +ABC chain extenders.High molecular weight PEA with intrinsic viscosity of 1.05 and 0.73 dL/g was obtained when PEA(90/10) and PEA(80/20) prepolymers were chain extended.The PEA prepolymers and the chain extended PEA were characterized by FTIR and()~1H-NMR spectroscopy,differential scanning calorimetry(DSC) and thermogravimetric analysis(TGA).()~1H-NMR spectra revealed that during the preparation of PEA prepolymers,ester-amide exchange side reaction took place.DSC studies indicated that after chain extension,the T_g of PEA(80/20) increased,and its ΔH_m as well as T_m decreased.PEA(0/100) is a non-crystallizable polyesteramide,and its T_g is 65℃.TGA studies showed that as the content of HETA used in the synthesis of PEA(x/y) prepolymers increased,the thermal stability of the prepolymers decreased,because the introduced terephthalic diesterdiamide showed less stability.
What problem does this paper attempt to address?