Effect of Milling Time on the Microstructure of Ti35Nb2 center dot 5Sn5HA Biocomposite Fabricated by Powder Metallurgy

Xiaopeng Wang,Yuyong Chen,Lijuan Xu,Shulong Xiao,Kee-Do Woo
2012-01-01
Abstract:A novel Ti-35Nb-2 center dot 5Sn/5Hydroxyapitite(HA) biocompatible composite was fabricated by pulsed current activated sintering (PCAS) at 1100 degrees C under 60 MPa. The raw powders were high energy mechanical milled (HEMM) for 0 h,4 h,8 h and 12 h. The effect of milling time on the morphologies of Ti35Nb2 center dot 5Sn/5HA powders and microstructures of composite were studied. Results indicated that ball milling for 8 h led to a phase starting to transform into beta phase and after milled for 12 h the powders contained only beta phase. After milled for 12 h, the particle size of the powders was about 200 nm and the grain size of sintered composite was about 50nm. As the increase of ball milling time both hardnesses and relative densities of the sintered composites were increased.
What problem does this paper attempt to address?