Abstract:TiC/Cu composites were prepared by means of high-energy ball mill and cold-press sintering. Confirming the better process parameters, the effects of the milling time and sintered temperature on microstructure, mechanical properties and electric conductivity of TiC/Cu composites was discussed. The shape of the composite grains changed from laminar to spherical and lattice distortion increased with the milling time increasing. The increase of the sintering temperature and TiC contents help to decrease porosity and density of the composites. With increasing of TiC mass fraction the bend strength increased first and then decreased,the peaks both appear in 10wt. %. The increasing of the sintering temperature is beneficial to improve the bend strength. Ball milled 15h the electric conductivity performs at optimum level. When the milling reached 24h, fine particles appear agglomeration and it shows a low level of the electric conductivity.
What problem does this paper attempt to address?