Characterization and Microstructural Evolution of Continuous BN Ceramic Fibers Containing Amorphous Silicon Nitride
Yang Li,Min Ge,Shouquan Yu,Huifeng Zhang,Chuanbing Huang,Weijia Kong,Zhiguang Wang,Weigang Zhang
DOI: https://doi.org/10.3390/ma14206194
IF: 3.4
2021-10-18
Materials
Abstract:Boron nitride (BN) ceramic fibers containing amounts of silicon nitride (Si3N4) were prepared using hybrid precursors of poly(tri(methylamino)borazine) (PBN) and polycarbosilane (PCS) via melt-spinning, curing, decarburization under NH3 to 1000 °C and pyrolysis up to 1600 °C under N2. The effect of Si3N4 contents on the microstructure of the BN/Si3N4 composite ceramics was investigated. Series of the BN/Si3N4 composite fibers containing various amounts of Si3N4 from 5 wt% to 25 wt% were fabricated. It was found that the crystallization of Si3N4 could be totally restrained when its content was below 25 wt% in the BN/Si3N4 composite ceramics at 1600 °C, and the amorphous BN/Si3N4 composite ceramic could be obtained with a certain ratio. The mean tensile strength and Young’s modulus of the composite fibers correlated positively with the Si3N4 mass content, while an obvious BN (shell)/Si3N4 (core) was formed only when the Si3N4 content reached 25 wt%.
materials science, multidisciplinary,chemistry, physical,physics, applied, condensed matter,metallurgy & metallurgical engineering