A Method to Form Well-Adhered Γ-Al2o3 Layers on FeCrAl Metallic Supports

S Zhao,JZ Zhang,D Weng,XD Wu
DOI: https://doi.org/10.1016/s0257-8972(02)00859-9
2003-01-01
Abstract:Well-adhered γ-Al2O3 coating layers can be formed on FeCrAl metallic supports for the preparation of structured catalysts in diesel particulate filter (DPF) systems using a three-step method—pre-oxidation, primer deposition and coating deposition. The optimal pre-oxidation is at 950 °C for 10 h; the optimal primer sol calcination is at 800 °C for 3 h; and the optimal γ-Al2O3 slurry calcination is at 900 °C for 2 h. If the oxidation temperature is 1050 °C, only 0.5 h is required to obtain almost the same coating adhesion level as at 950 °C for 10 h. The data concerning effects of the major preparation parameters (the pre-oxidation time, temperature, primer calcination temperature and the coating calcination temperature) are presented herein. The coating adhesion was measured by ultrasonic adhesion, thermal shock and interface shear strength tests.
What problem does this paper attempt to address?