2Si-B-3c-n Ceramics Prepared by Mechanical Alloying and Hot-Pressing Consolidation

Yang Zhihua,Duan Xiaoming,Jia Dechang,Zhou Yu
DOI: https://doi.org/10.3321/j.issn:1002-185x.2009.z2.040
2009-01-01
Rare Metal Materials and Engineering
Abstract:25i-B-3C-N powders were prepared by mechanical alloying with Si3N4, B4C, C and Si as starting materials and they were hot pressed at 1900 degrees C under 40 MPa for 30 min in N-2 atmosphere to obtain 25i-B-3C-N ceramic. Microstructure and mechanical properties of the bulk ceramic were studied. After hot pressing the density of the powder was up to 97.9%. The HPed ceramic was mainly composed of equiaxed beta-SiC and lamellar h-BCN phase. The size of BCN grains was about 200 nm and that of SiC about 400 similar to 500 nm. BCN grains distributed around SiC grains. The flexural strength, elastic modulus, fracture tough and Vickers hardness were 446.6 MPa, 144.6 GPa, 5.10 MPa1/2 and 5.53 GPa, respectively. In air atmosphere at high temperature, the flexural strength decreased as the temperature increasing, which was 358.7 MPa and 202.1 MPa at 1000 degrees C and 1400 degrees C, respectively.
What problem does this paper attempt to address?