Preparation of calcium carbonate and nesquehonite (MgCO3·3H2O) from low-grade magnesite

Qiyan Shan,Yue Zhang,He Yang,Xiangxin Xue
2011-01-01
Abstract:Calcium carbonate and nesquehonite were prepared using low-grade magnesite as raw material. Firstly, the low-grade magnesite was calcined, and then reacted with ammonium chloride solution to obtain CaCO3 and the solution of MgCl2. Finally, nesquehonite was precipitated from the solution of MgCl2 by using ammonium carbonate as precipitant. The results showed that with 1% of MgCl2·6H2O as additive, the low-grade magnesite was calcined at 650°C for 2h, thus the calcined product was mainly composed of CaCO3 and MgO. The influences of process conditions on the dissolution rate of magnesium were investigated, and the results showed that the optimal process conditions were: 80°C for 60min, the excess coefficient of ammonium chloride was 30%, and the ratio of liquid to solid was 8 through two-step leaching, under which the dissolution rate of magnesium was 92%, and leaching residue was mainly composed of CaCO3. Nesquehonite with a diameter of 1-3μm and a length of 15-20μm obtained as precipitation reaction temperature was 37°C, the excess coefficient of ammonium carbonate was 50%, and aging time was 2h. In addition, the purity of nesquehonite was 96.5%.
What problem does this paper attempt to address?