Preparation Technology of Sr_2MgSi_2O_7∶Eu~(2+),Dy~(3+) Luminous Materials and Their Luminous Performance

Qi Xiaoxia,Zhao Junwu,Feng Yi
2006-01-01
Abstract:The Sr2MgSi2O7∶Eu2+,Dy3+ luminous materials were synthesized by solid sintering technology at the presence of carbon as reductant.The factors that influence the luminous performance and preparation technology were discussed.These luminous materials exhibited broadband peaks in both the excitation and emission spectra.The excitation peaks lied between 220 and 450 nm,and the main emission peaks lied around 463 nm.The results indicate that the luminescence of these materials are due to 4f7(8S7/2)-4f65d transition of Eu2+.Additionally,the long afterglow of the Sr2MgSi2O7∶Eu2+,Dy3+ luminous materials can last over 10 h in the light perception of the human eye.Its luminescence decay consisted of the initial fast process and the later extremely slow process.Effects of such factors as the temperature in the sintering process,different proportions of Eu/Dy and different additions of boracic acid on the relative luminescent intensity were studied.
What problem does this paper attempt to address?