Eu AND Dy CO-DOPED Sr2MgSi2O7-BASED LONG AFTERGLOW PHOTOLUMINESCENT MATERIALS

王晓欣,林元华,张中太
DOI: https://doi.org/10.3321/j.issn:0454-5648.2002.02.016
2002-01-01
Abstract:Long afterglow photoluminescent materials Sr 2MgSi 2O 7∶Eu, Dy were prepared by sintering in reductive atmosphere at high temperature. The luminescent properties and phosphorescent mechanism of Sr 2MgSi 2O 7_based luminescent phosphor were studied. The analytical results indicated that the emission spectra of Sr 2MgSi 2O 7: Eu, Dy lied in near 469 nm, resulted from the transition of 4 f5d-4f of Eu 2+ ions. Co_doped Dy 3+ produced suitable depth energy traps, which improved afterglow property dramatically. Its initial luminescent intensity reached 2 200 mcd/m 2 and the duration time lasted over 5 h.