Low‐Temperature Sintering and Microwave Dielectric Properties of Ba3(VO4)2–BaWO4 Ceramic Composites

Hao Zhuang,Zhenxing Yue,Siqin Meng,Fei Zhao,Longtu Li
DOI: https://doi.org/10.1111/j.1551-2916.2008.02672.x
IF: 4.186
2008-01-01
Journal of the American Ceramic Society
Abstract:New low‐temperature co‐fired microwave dielectric composites with compositions of (1–x)Ba3(VO4)2–xBaWO4 (x=0–1) were prepared by firing mixtures of Ba3(VO4)2 and BaWO4. Thermal mechanical analysis indicated the ceramic composites had relatively low densification temperatures and could be sintered in the temperature range 925°∼950°C. X‐ray diffraction patterns showed that Ba3(VO4)2 and BaWO4 coexisted and no secondary phase was detected in the sintered bodies, implying good chemical compatibility between the two phases. Near‐zero temperature coefficients of the resonant frequency (τf) could be achieved by changing the relative content of the two phases, due to their positive and negative τf values, respectively. With increasing BaWO4 (x from 0.50 to 0.65), the τf value of the composites decreased from +10.9 to −1.9 ppm/°C, and the quality factor (Q×f value) increased from 66 700 to 79 100 GHz. The best microwave dielectric properties were obtained for x=0.65 samples sintered at 925°C with a dielectric constant of 11.1, a Q×f value of 79 100 GHz, and a τf value of −1.9 ppm/°C. Chemical compatibility experiments showed the ceramics are compatible with silver during cofiring process.
What problem does this paper attempt to address?