Abstract:Surface-treated aluminum hydroxide(ATH) and magnesium hydroxide(MH) mixture(SAMH),linear low density polyethylene(LLDPE) and polyethylene grafted by maleic anhydride(PE-MAH) were melt-kneaded and extruded to produce a flame-retardant masterbatch,and then was extruded with polyamide 6(PA6) to yield PA6/SAMH/PE(50/30/20 by mass ratios)ternary composite.The composite via masterbatch method passed UL94 V-0@3.2mm in vertical burning testing and the limiting oxygen index(LOI) attained 33.0%.The impact strength was twice of PA6/SAMH binary system with a same flame-retarded performance.The flame-retardancy of the composite was poor when all compositions were extruded synchronously.The flame-retarded mechanism of the ternary composites was investigated by thermogravimetric analysis(TGA) and scanning electronic microscope(SEM).It was found that a preferential interaction at the boundary between SAMH particles and PA6/PE polymer host of the composite via masterbatch method resulted in the occurrence of a compact burning carbon layer and a high carbon residue.
What problem does this paper attempt to address?