Abstract:Three kinds of new barrier films were introduced on the surface of Ca60Mg15Zn25 bulk metallic glasses (BMGs) in order to slow down its biodegradation/corrosion rate, including fluoroalkylsilane (FAS) coating, pure Fe film and (Fe+FAS) bilayer. The changes of surface morphology were characterized by scanning electron microscopy (SEM). Contact angle meter was applied to test the surface wettability at ambient temperature. The corrosion rate was investigated by immersion test in deionized water. It was found that various micro-nanoscale hierarchical structures could be constructed after different surface treatments. By suitable surface modification strategy, Ca60Mg15Zn25 BMG showed increased water contact angle even up to 133.6°. The immersion experiment results showed that Fe film and FAS thin film coatings with hydrophobic and insulative characteristics are beneficial to provide effective anti-corrosive protection to Ca60Mg15Zn25 BMG, with the sequence: Fe coating>(Fe+FAS) treated>FAS treated.
What problem does this paper attempt to address?