Process and Structure Research on Preparation of Mn-Zn Ferrite by Co-precipitation and Oxides Methods

罗广圣,李建德,周正有,姜贵文,李文善
DOI: https://doi.org/10.3969/j.issn.1006-0456.2009.04.021
2009-01-01
Abstract:Taking the zinc oxide,manganese sulfate and ferric nitrate as the main raw materials,using chemistry co-precipitation method to prepare Mn-Zn ferrites forerunner body powder,we can prepare Mn-Zn ferrites together with the precursor powder which takes the ferric oxide,zinc oxide and manganese dioxide as the main raw materials through traditional oxide solid-phase sintering.Through analyzing the structure of crystal structure,microstructure and thermal properties of the samples,the samples sintered are showed a good spinel ferrite.Sintering the samples which were prepared by co-precipitation at 1 250 ℃ for 4 hours,the crystal grain is tiniest,and the Curie temperature and density achieves in a big way.Sintering the samples which were prepared by co-precipitation at 1 280 ℃ for 4 hours,the solid-phase reaction is the most complete.Sintering the samples which were prepared by traditional method at 1 220 ℃,the reaction with Fe2O3 which generated Mn-Zn ferrites with spinel structure is the most complete.The samples' unit cell volumes by the co-precipitation and oxides methods have an inflation compared to the theory value.When 1 250 ℃,the crystal constant and the unit cell volume are smallest.
What problem does this paper attempt to address?