Preparation and properties of nitrile rubber/nylon 12 thermoplastic elastomer by dynamic vulcanization

Xing Lihua,Wu Shemao,Zhang Liqun
DOI: https://doi.org/10.3969/j.issn.1000-1255.2010.03.011
2010-01-01
Abstract:The nitrile rubber(NBR)/nylon 12(PA 12) thermoplastic elastomers(TPE) were prepared by dynamic vulcanization.The curing time was determined by Haake internal mixer,and the morphological structure was characterized.The effects of NBR/PA 12(mass ratio) and plasticizer types on the properties of TPE were investigated,and the TPE was analyzed by differential scanning calorimetry.The results showed that the TPE behaved as two-phase structure with PA 12 as continuous phase and NBR as dispersed phase.With increasing the PA 12 amount,the tensile strength and oil resistance increased obviously,and the Shore A hardness and compression set increased as well,elongation at break initially decreased and then increased,and the appropriate mass ratio of NBR/PA 12 was 70/30-60/40.The Shore A hardness decreased and elongation at break increased with the addition of dioctyl phthalate,liquid nitrile rubber and polypropylene adipate plasticzers,but the oil resistance was not affected.The melting point of TPE was higher than that of PA 12,and the melting enthalpy was lower than that of PA 12.
What problem does this paper attempt to address?