Surface Protection of Friction Stir Welding Joint of 5083 Aluminum Alloy by Micro-Arc Oxidation

鲁亮,薛文斌,金小越,杜建成,李永良
DOI: https://doi.org/10.13289/j.issn.1009-6264.2011.11.027
2011-01-01
Abstract:A ceramic coating on friction stir welding(FSW) joint of 5083 aluminum alloy was prepared by micro-arc oxidation(MAO) method.Morphology,phase constituent and microhardness of the MAO coating were analyzed by SEM,XRD and hardness test.The effect of MAO coating on corrosion property of the welded joint was evaluated by immersion test.The results show that the MAO coating on the FSW joint is uniform and compact.Microhardness of the FSW joint is lower than that of 5083 base alloy,however,microhardness of the MAO coating is one order of magnitude higher than that of aluminum alloy substrate,meanwhile the microhardness of the coating at different zones is the same.It is also found that after three days immersion in 0.2 mol/L NaHSO3 + 0.6 mol/L NaCl solution,pitting corrosion occurs on the surface of uncoated alloy,while the corrosion was not observed on the coated alloy.
What problem does this paper attempt to address?