Leaching zinc oxide ore in alkaline solution

ZHAO Zhong-wei,JIA Xi-jun,CHEN Ai-liang,LONG Shuang,HUO Guang-sheng,LI Hong-gui
2010-01-01
Abstract:To achieve the circulatory leaching of zinc oxide ores, the Bayer process was used to treat bauxite to zinc hydrometallurgy. The zinc oxide ores were leached in concentrated alkaline solution. When the temperature decreased, zinc was precipitated in the form of zinc hydroxid from solution. The concentrated mother liquor was returned to leach the zinc oxide ores, and the alkaline leaching process of zinc oxide ore was researched. The results show that under the condition of sodium hydroxide solution 5 mol/L, leaching temperature 85 ℃, liquid-solid ratio 101 and leaching time 2 h, the recovery rates of zinc, lead, and cadmium reach 77%, 9% and 5%, respectively.