The research of microtensile bond strength between core build-up composite modified with Ultrafine Diamond and fibre posts

PENG Juan-hong,LIU Xue-heng,PENG Dong,WANG Xin-zhi
2007-01-01
Abstract:Objective: To evaluate the microtensile bond strength (μTBS ) between two kinds of core build-up composites (Ultrafine Diamond Core, UFD-C; Luxa Core, L-C) and three types of fiber posts in vitro. Methods: For the microtensile nontrimming technique, 15 beam-shaped specimens per group were obtained from cylinders of core material which had been built up by progressively adding small increments of composite resin around the post. Each specimen was loaded in tension until failure and the interfaces present was observed. Results: The mean value(SD)on μTBS of UFD-C was 20.08(2.79)MPa for quartz fiber post, 17.78(5.70)MPa for glass fiber post, and 20.12(3.78)MPa for carbon fiber post. The mean value(SD)on μTBS of L-C was 21.09(3.64)MPa for group quartz fiber post, 23.55(3.41)MPa for group glass fiber post, and 18.12(3.80)MPa for carbon fiber post. There were no significant differences of the μTBS between UFD-C and L-C to quartz fiber post and carbon fiber post (P >0.05). The μTBS of L-C to glass fiber post was significantly higher than that of the UFD-C to glass fiber post (P <0.05). 92% of the was fracture mode adhesive failure. Conclusions: Ultrafine Diamond Core was as suitable for restoration of defected teeth with quartz fiber post and carbon fiber post as commercial core materials.
What problem does this paper attempt to address?