Effect of Reinforcement on High-temperature Flexural Strength of Silica-based Ceramic Cores

ZHAO Xiantao,CHENG Laifei,ZHANG Litong,DUO Guiying
DOI: https://doi.org/10.3969/j.issn.1001-3814.2012.01.001
2012-01-01
Abstract:The silica-based ceramic cores were strengthened by ethyl silicate hydrolysates and yttrium chloride solution.The results show that,the ceramic core samples strengthened by the hydrolysates of ethyl silicate can quickly generate much cristobalite at 1550 ℃,which can prohibite the viscous flow of the ceramic cores.The flexural strength is improved by nearly 50%.The ceramic core samples strengthened by the yttrium chloride solution are greatly softened,and almost has no bonding strength before 1500 ℃.
What problem does this paper attempt to address?