Comparison of anti-ozone aging properties of three silicone rubbers for maxillofacial prosthese

Han Ying,Zhao Yi-min,Lu Yi,Shao Long-quan
DOI: https://doi.org/10.3969/j.issn.1673-8225.2010.51.026
2010-01-01
Abstract:BACKGROUND:Exposed in air for long time,maxillofacial silicone prosthese will be effected by many factors,such as light,heat and ozone.The effect of these factors will make the mechanical properties of prostheses be worse than before,which cause that silicone rubbers change color and become hard,crisp and sticky.The physical and mechanical properties gradually reduce,manifested as decreased strength and disappeared flexibility,eventually leading to loss of use value.OBJECTIVE:To compare the mechanical properties of three silicone rubbers before and after ozone aging (ZY-1,SY-1,A-2186),and to evaluate the anti-ozone aging properties of ZY-1 silicone elastomer.METHODS:The mechanical properties of three silicone rubbers were tested before and after ozone aging in accordance with GB/T 7762-1987 "Vulcanized rubber static tensile method of anti-ozone aging test".Statistical analyses were done using a two-way analysis of variance.RESULTS AND CONCLUSION:After ozone aging,the tensile strength,the elongation at break and tear resistance of three silicone rubbers reduced,while the hardness and permanent deformation rate increased.The percentages of elongation at break and tear resistance,as well as shore A hardness,of ZY-1 were significantly lower than that of SY-1 (P<0.05),and similar to that of A-2186 (P>0.05).ZY-1 addition-type silicone rubbers can maintain good flexibility and hardness,have reasonable anti-ozone aging properties.
What problem does this paper attempt to address?