Abstract:SrBi8Ti7O27 ferroelectric ceramics with mixed Aurivillius structure were modified by La-substitution for Bi, and the dielectric properties were investigated together with the microstructure characterization. Solid solution of Sr(Bi1 − xLa x )8Ti7O27 was formed in the present ceramics for x ≤ 0.1, and (Bi,La)4Ti3O12 secondary phase appeared at x = 0.15. For x ≥ 0.25, another phase Sr(Bi,La)4Ti4O15 appeared, and (Bi,La)4Ti3O12 disappeared gradually with increasing x, and vanished entirely at x = 0.35. With increasing x, both the dielectric constant and dielectric loss of the present ceramics increased firstly and reached their maximums 291 and 0.023 at 1 MHz, then decreased after x > 0.25. The temperature stable high-ε dielectric ceramics with low dielectric loss were created at the composition x = 0.5: ε = 122, tan δ = 0.0003 and τε = −619 ppm/°C at 1 MHz.
What problem does this paper attempt to address?