Glassy and Icosahedral Phases in Rapidly Solidified Ti–Zr–Hf–(Fe, Co or Ni) Alloys

N Chen,DV Louzguine-Luzgin,S Ranganathan,A Inoue
DOI: https://doi.org/10.1016/j.jnoncrysol.2005.06.041
IF: 4.458
2005-01-01
Journal of Non-Crystalline Solids
Abstract:The icosahedral quasicrystalline, amorphous plus crystalline and glassy phases were formed in Ti40Zr20Hf20(3d-LTM)20 alloys (3d-LTM=3d late transition metals Fe, Co and Ni). The icosahedral phase formed in the melt-spun Ti40Zr20Hf20Fe20 alloy is metastable and the average size of the quasicrystalline icosahedral particles precipitated in the amorphous matrix is 5nm. The metastable icosahedral phase transformed to a big-cubic fcc Hf2Fe phase with the grain size of about 20nm after annealing for 1.8ks at 841K. The glassy phase was formed in the melt-spun Ti40Zr20Hf20Co20 alloy and no metastable phase was found to form during the transformation from glassy phase to a stable crystalline phase. Icosaheadral phase formed in the melt-spun Ti40Zr20Hf20Ni20 alloy transformed to a big-cubic fcc (Zr,Ti)2Ni solid solution phase by a solid state reaction.
What problem does this paper attempt to address?