Study on preparation of fly ash water permeable brick

RAO Lingli,CAO Jianxin,ZHANG Hongbo,YANG Lin,PANG Ying,LIU Yi,WANG Jingjing
DOI: https://doi.org/10.3969/j.issn.1001-702X.2006.07.016
2006-01-01
Abstract:Study is made on preparation of water permeable brick using fly ash as main raw material. The influence of forming pressure, burn system and the grain size of aggregates on compressive strength and permeability of the product are discussed. The result indicates that proper process parameters are as follows: fly ash 40%~50%, clay 25%~35%, waste floor tile 20%~30% with grain size 0.45~0.6 mm, forming pressure 25 MPa, firing temperature 1 050 ℃, temperature holding time 1h. The compressive strength and coefficient of water permeability of the fly ash water permeable brick is 30.6 MPa and 1.08×10-2 cm/s respectively that meet the requirement of Chinese standard JC/T 945-2005 "water permeable brick".