Sintering Process of Diasporic Bauxite with High Iron Content at Low Ratio of Lime to Silica for Alumina Production

刘桂华,张明,肖伟,彭志宏,周秋生,李小斌
DOI: https://doi.org/10.3321/j.issn:1004-0609.2008.10.024
2008-01-01
The Chinese Journal of Nonferrous Metals
Abstract:The sintering process of diasporic bauxite with high iron content was studied. The results show that 3CaO·2SiO2, and 2CaO·SiO2, are primarily formed in the sintering process when diasporic bauxite is sintered at soda ratio Na2O/(Al2O3+Fe2O3) of 1 and lime ratio CaO/SiO2 of 1.5. The increase of n(CaO)/n(SiO2) decreases the extraction of alumina and silica. The prolongation of sintering time and the increase of sintering temperature benefit the alumina extraction but reduce the silica extraction. The increase of the ratio of iron to alumina decreases the sintering temperature and narrows the sintering temperature range. The results from the Al2O3 available extraction rate also indicate that the high alumina extraction rate can be obtained at n(CaO)/n(SiO2) of 1.5. The feasible technology for sintering is as follows: sintering temperature 1 250-1 300 ℃, sintering time 20-40 min, n(CaO)/n(SiO2) of 1.5.
What problem does this paper attempt to address?