RESEARCH ON THE EXTRACTIONOF AMORPHOUS SiO2 FROM HIGH-ALUMINIUM FLY ASH

Zhan-jun ZHANG,Jun-min SUN,Qiang YAO,ying HE,Hong-wen MA
DOI: https://doi.org/10.3321/j.issn:1000-4734.2007.02.008
2007-01-01
Abstract:In order to increase the Al/Si ratio of high-aluminium fly ash,so as to lay a foundation for the extraction of Al2O3,this paper focuses on how to effectively extract SiO2 from fly ash as well as on the reaction mechanism.Firstly,according to the chemical and mineralogical composition of the fly ash,the technical route of extracting amorphous SiO2 by NaOH was determined.Then,the optimum extraction conditions were determined by orthogonal experiments and necessary complementary experiments.The optimum conditions are presented as follows: concentrations of NaOH: 25%;mass ratio of ash to alkali:1∶0.5;reaction temperature: 95 ℃,and reaction time: 4 hours.After reaction under the optimum conditions,the extraction efficiency of SiO2 amounts to 41.8%,the Al2O3 contents of the fly ash increase from 48.5% to 57.38% and Al2O3/SiO2 mass ratio increases from 1.29 to 2.39.
What problem does this paper attempt to address?