Synthesis, Structure, and Color-Tunable Luminescence Properties of Lanthanide Activator Ions Doped Bismuth Silicate As Single-Phase White Light Emitting Phosphors
Lei Zhang,Pan Li,Ankang Zhao,Xiao Li,Jie Tang,Fangbo Zhang,Guang Jia,Cuimiao Zhang
DOI: https://doi.org/10.1016/j.jallcom.2019.152546
IF: 6.2
2019-01-01
Journal of Alloys and Compounds
Abstract:A series of lanthanide activator ions (Ln(3+)) doped bismuth silicate Bi4Si3O12 phosphors have been fabricated via the Pechini sol-gel route. The as-synthesized eulytite structured Bi4Si3O12 sample which exhibits intense green-blue emission is beneficial for host materials of lanthanide activator ions. When the Ln(3+) ions (Sm3+, Dy3+, or Eu3+) are doped into the Bi4Si3O12 host, an insufficient energy transfer occurs from the host matrix to Ln(3+) ions, which can be confirmed by the photoluminescence spectra and decay lifetimes of the Ln(3+) doped samples. The as-synthesized Bi4Si3O12:Ln(3+) phosphors show both the intrinsic broad band luminescence of Bi4Si3O12 host and the characteristic sharp peak emissions of Ln(3+) ions, which can generate the tunable multicolor emissions in a single-phase phosphor by adjusting the Ln(3+) doping concentrations. More importantly, three kinds of Ln(3+)-doped single-phase white light emitting phosphors with excellent chromaticity coordinate (x, y) and CCT in the warm white region [Sm3+: (0.336, 0.330), 5315 K; Dy3+: (0.330, 0.370), 5614 K; Eu3+: (0.340, 0.307), 5034 K] can be obtained when the doping concentrations of Sm3+, Dy3+, and Eu3+ are fixed at 0.5, 5, and 1 mol%, which are quite close to the daily use of pure white light. By integrating the Bi4Si3O12:Ln(3+) phosphors into a 280 nm UV LED chip, all the fabricated WLED devices can exhibit bright white light emission, which provides direct evidence that the as-synthesized BSO:Ln(3+) (Ln = Sm, Dy, and Eu) single-phase white-emitting phosphors have great potential for WLEDs and optoelectronic devices. (C) 2019 Elsevier B.V. All rights reserved.