Studies on hardness, elastic modulus and high temperature oxidation resistance of TiC and TiB 2 dispersed titanium aluminide (Ti45Al5Nb0.5Si) composites developed by laser direct energy deposition

Anupama Dutta,Andreas Weisheit,Tapas Bera,Jyotsna Dutta Majumdar
DOI: https://doi.org/10.1016/j.corsci.2024.112555
IF: 7.72
2024-11-06
Corrosion Science
Abstract:In this study, TiC (5 to 10 wt.%) and TiB 2 (5 to 10 wt.%) reinforced TiAl (Ti45Al5Nb0.5Si) composites have been developed by laser direct energy deposition (LDED) process. The microstructures of TiAl/TiC and TiAl/TiB 2 composites consist of TiC and TiB 2 particles dispersed in γ and α 2 matrix. The microhardness of the composites is improved from 571 HV to 634-683 HV (for TiC dispersion) and 649-694 HV (for TiB 2 dispersion). The activation energy of cyclic oxidation is increased from 228 kJ/mol (Ti45Al5Nb0.5Si) to 271-301 kJ/mol (TiC dispersion) and 262-296 kJ/mol (TiB 2 additions). The mechanism of oxidation of the composites is established.
materials science, multidisciplinary,metallurgy & metallurgical engineering
What problem does this paper attempt to address?