One Stone for Multiple Birds: A Versatile Cross-Linked Poly(dimethyl siloxane) Binder Boosts Cycling Life and Rate Capability of an NCM 523 Cathode at 4.6 V

Xiaoying Fan,Peng Chen,Xu Yin,Ruo-Xuan Qi,Chao Yang,Ya-Jun Cheng,Kunkun Guo,Cuirong Liu,Yonggao Xia
DOI: https://doi.org/10.1021/acsami.2c01245
2022-03-30
Abstract:Increasing working voltage is a promising way to increase the energy density of lithium-ion batteries. Cycling and rate performance deteriorated due to excessive electrolyte decomposition and uncontrolled formation of a cathode–electrolyte interface (CEI) layer at a high voltage. A new concept is proposed to construct a high-voltage-stable electrode–electrolyte interface. An elastomeric poly(dimethyl siloxane) (PDMS) binder is incorporated into the electrode to modify the LiNi0.5Co0.2Mn0.3O2 (NCM 523) particle surface via an in situ cross-linking reaction between hydroxy-terminated PDMS and methyl trimethoxy silane promoted by moisture at ambient conditions (MPDMS). Improved electrochemical performance is achieved with the MPDMS binder in terms of reversible capacity (201 vs 185 mAh·g–1 at 0.2C), capacity retention (80 vs 68%, after 300 cycles at 1C), and rate performance (55.6% increase at 5C), as demonstrated by the NCM 523||Li half-cell. The NCM 523||graphite full-cell also shows improved performance at 4.6 V (147 vs 128 mAh·g–1, 82 vs 76%, after 200 cycles at 1C). The mechanism studies indicate that MPDMS exerts multiple effects, including cathode surface passivation, solvation structure tuning, electrolyte uptake enhancement, and mechanical stress relief. This work provides an inspiring route to realize high-voltage application of lithium-ion battery technology.The Supporting Information is available free of charge at https://pubs.acs.org/doi/10.1021/acsami.2c01245.Viscosity changes of NCM-PVDF and NCM-MPDMS/PVDF electrode slurries at different shear rates; cross-sectional SEM images of NCM-PVDF and NCM-MPDMS/PVDF electrode applied with ion polishing after 100 cycles; discharge specific capacity of the NCM-PVDF and NCM-MPDMS/PVDF electrodes at different voltages with different current densities; cycling and rate performance of the NCM-PVDF and NCM-MDMS/PVDF electrodes between 2.8 and 4.3 V; SEM images of NCM-PVDF and NCM-MPDMS/PVDF electrodes before cycling; cross-section SEM images of the NCM-PVDF and NCM-MPDMS/PVDF electrodes after 100 cycles via ion polishing treatment; TEM images of NCM 523 pristine particles, NCM-MPDMS/PVDF, and NCM-PVDF electrodes before cycling; EDS images of NCM-PVDF NCM-MPDMS/PVDF electrodes before and after 100 cycles; the electrochemical impedance (EIS) profiles of the cells measured at different cycles and canning voltammetry curves at different sweep rates between 2.8 and 4.6 V for NCM-PVDF and NCM-MPDMS/PVDF electrodes; C 1s spectrum of the NCM-PVDF and NCM-MPDMS/PVDF electrodes before and after 100 cycles; Ni 2p XPS spectra of the NCM-PVDF and NCM-MPDMS/PVDF electrodes after 100 cycles; active adsorption sites of lithium ions in PDMS, PVDF, EC, and DMC and their corresponding adsorption energies (PDF)This article has not yet been cited by other publications.
materials science, multidisciplinary,nanoscience & nanotechnology
What problem does this paper attempt to address?