Effect of Vacuum Carburizing Time on Microstructure and Mechanical Properties of Tantalum Carbide Layer

Chongqing Di,Xiaodong Yan,Xuming Lv,Chao Yan,Wei Ye,Defu Li
DOI: https://doi.org/10.1007/s12540-020-00934-z
IF: 3.451
2021-02-01
Metals and Materials International
Abstract:<span class="a-plus-plus abstract-section id-a-sec1"><p class="a-plus-plus">A (TaC/Ta<sub class="a-plus-plus">2</sub>C) carbide bilayer is obtained by vacuum carburizing technology on the surface of Ta substrate at 1673 K for 4, 8, and 12 h. XRD, SEM and EBSD are utilized to investigated phase composition and the microstructure. The mechanical properties of the Ta and tantalum carburized materials are studied with Vicker's hardness tester and nanoindenter, adhesion automatic scratch tester, reciprocating friction and wear testing machine. The results show that the outside surface phase composition of the carbide bilayer is all the TaC phase. With the increase of the carburizing time from 4 to 12 h, the average grain size from approximately 500 nm to 10 μm, the thickness of the carbide bilayer is from 11 to 20 μm. The microhardness increases from 104.1 to 322.5 HV, and the elastic modulus are from 466.6 to 615.3 GPa. Adhesive strength is best at 8 h, 49.1 N, compared to 19 N at 4 h and 36.5 N at 12 h. The friction and wear coefficient of Ta fluctuates significantly between 0.6 and 1.0, after carburizing treatment, the friction and wear coefficient fluctuates smoothly, and the wear resistance is well improved.</p></span><span class="a-plus-plus abstract-section id-a-sec2 outputmedium-online"><h3 class="a-plus-plus">Graphic </h3></span>
materials science, multidisciplinary,metallurgy & metallurgical engineering
What problem does this paper attempt to address?