Influence of the sintering method on microstructure and microhardness of AlCuNiSnZn-based high-entropy brasses and bronzes obtained by powder metallurgy

L.D. Laguna-Zubia,C.G. Garay-Reyes,P.A. Guerrero-Seañez,M.A. Ruiz-Esparza-Rodríguez,J.M. Mendoza-Duarte,I. Estrada-Guel,S. González,A. Martinez-Garcia,R. Martínez-Sánchez
DOI: https://doi.org/10.1016/j.vacuum.2024.113006
IF: 4
2024-01-28
Vacuum
Abstract:The present report focused on synthesizing and characterizing a series of AlCuNiSnZn alloys obtained by powder metallurgy as a new family of high-entropy brasses and bronzes. The (AlCuNi) 80 Sn 10 Zn 10 and (AlCuNi) 70 Sn 15 Zn 15 alloys were obtained by mechanical alloying and sintering, evaluating two sintered methods: high-frequency induction heat and conventional. After 10 h of mechanical alloying, the elemental powder mixture formed solid solutions of face-centered cubic (FCC-α) and body-centered cubic (BCC-β) phases. However, the solid solutions, after sintering, were decomposed into a mixture of γ Ni 2 Zn 11 , AlNi, and Cu 2 Ni 3 Sn 3 phases. The (AlCuNi) 80 Sn 10 Zn 10 system sintered by high-frequency induction heat exhibits a microhardness value of ∼501 HV±17, while that obtained by the conventional method was ∼320 ± 21 HV. The results showed that it is convenient to maintain the BCC/FCC solid solutions after sintering due to their stability and properties. In addition, it is necessary to design alloys with lower values of ΔH mix to improve the microhardness.
materials science, multidisciplinary,physics, applied
What problem does this paper attempt to address?