Structure and magnetic properties of anisotropic bulk TbCu7-type (Sm, Pr)Co7 nanocrystalline magnets

Yingxin Hua,Li Lou,Bo Jiang,Jianyuan Kou,Jinyi Wang,Jieqiong Gao,Tiancong Li,Qian Zhang,Xiaohong Li
DOI: https://doi.org/10.1016/j.jmmm.2020.167415
IF: 3.097
2021-01-01
Journal of Magnetism and Magnetic Materials
Abstract:Fabricating anisotropic bulk TbCu7-type RCo7 nanocrystalline magnets is of great significance for their development as high-performance high temperature magnets. In this paper, anisotropic bulk TbCu7-type (Sm0.6Pr0.4)Co7 nanocrystalline magnets have been prepared using high-pressure thermal compression (HPTC). The (Sm0.6Pr0.4)Co7 magnet had a strong (002) crystallographic texture and a small grain size of ~20 nm, yielding a maximum energy product of (BH)max = 19.5 MGOe. The magnets showed a coercivity temperature coefficient of β = −0.21%/°C from room temperature (RT) to 300 °C, better than that −0.23%/°C of the SmCo7 magnets prepared in the same conditions.
materials science, multidisciplinary,physics, condensed matter
What problem does this paper attempt to address?
The paper attempts to address the problem of preparing anisotropic bulk nanocrystalline TbCu7-type (Sm,Pr)Co7 permanent magnets with high temperature stability and high performance. Specifically, the researchers aim to prepare (Sm0.6Pr0.4)Co7 nanocrystalline permanent magnets with strong (002) crystal texture and small grain size (about 20 nanometers) using high-pressure thermal compaction (HPTC) technology to realize their potential for high-temperature applications. ### Main Research Background: 1. **Demand for High-Temperature Permanent Magnets**: Rare-earth cobalt-based (RCo) permanent magnets have garnered widespread attention for their potential applications in high-temperature environments. Compared to RCo5 and R2Co17, RCo7 (R = Sm, Pr) possesses higher saturation magnetization (Ms), anisotropy field (HA), Curie temperature (Tc), and a lower temperature coefficient of coercivity (β), making it a candidate material for the next generation of high-temperature permanent magnets. 2. **Challenges in Preparation**: RCo7 is a metastable phase, posing stability issues during preparation. Typically, a third element is added to enhance its stability, but this often reduces Ms or Tc, thereby affecting magnetic performance. 3. **Impact of Grain Size and Texture**: Reducing the grain size to a critical value can effectively stabilize the metastable phase, but achieving oriented grain alignment remains a challenge. ### Research Objectives: - **Preparation Method**: To prepare (Sm0.6Pr0.4)Co7 nanocrystalline permanent magnets with strong (002) crystal texture and small grain size using high-pressure thermal compaction (HPTC) technology. - **Performance Optimization**: To optimize magnetic performance, particularly the maximum energy product ((BH)max) and the temperature coefficient of coercivity (β). - **High-Temperature Stability**: To evaluate the magnetic performance of the prepared magnets in high-temperature environments, especially coercivity and Curie temperature. ### Main Achievements: - **Successful Preparation**: Successfully prepared (Sm0.6Pr0.4)Co7 nanocrystalline permanent magnets with strong (002) crystal texture and about 20 nanometers grain size using HPTC technology. - **Excellent Magnetic Performance**: The maximum energy product of the magnet reached 19.5 MGOe, with a temperature coefficient of coercivity of -0.21%/°C, superior to SmCo7 magnets prepared under the same conditions. - **High-Temperature Stability**: The Curie temperature reached as high as 840°C, indicating its potential for high-temperature applications. ### Significance: These research findings provide important theoretical and technical support for the development of high-performance anisotropic bulk nanocrystalline (Sm,Pr)Co7 permanent magnets suitable for high-temperature environments, and are expected to promote the development and application of high-temperature permanent magnet materials.