Machinability and pulse characteristics of Ti-16Al-14Nb (α/β) alloy in wire-electric discharge machining process: A surface integrity study
K. Veera Venkata Nagaraju,M. Joseph Davidson,G. Venkatesh,M. Manjaiah,K. Harikrishna
DOI: https://doi.org/10.1177/09544089241255942
2024-05-25
Proceedings of the Institution of Mechanical Engineers Part E Journal of Process Mechanical Engineering
Abstract:Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering, Ahead of Print. The goal of the present work is to produce the efficient cutting of Ti-16Al-14Nb (α/β) alloy through wire-electric discharge machining and contemplate the terminologies such as machining ability, surface integrity and material removing capability. For this, the experimentation has been designed by considering three process parameters, pulse-on time (Ton), pulse-off time (Toff) and peak current (Ip) at three significant levels (low, high, intermediate) in L27 order designed from design of experiments. The effect of these process variables on pulse characteristics, surface roughness (Ra), kerfwidth (Kw) and material removal rate (MRR) is analyzed and mathematically modeled with analysis of variance. The results state that the highest MRR (0.521, 0.51, 0.506 mm3/sec) and low surface roughness (8.91, 8.89, 8.68 μm) values are observed at the highest level (110 μs, 15 μs, 8 A). If the pulse duration is kept at low (Ton = 40μs, Toff = 3μs), the increase in peak current from 3 A to 8 A leads to a 64.54% increase in MRR and a 52.9% increase in Ra values. ANOVA results stated that Ton has contributed 20.4%, 35.8% and 19.3%, and Ip has contributed 43.1%, 30.5% and 46.6% influence on MRR, Kw and Ra respectively. The voltage–current characteristics studies confirmed that the strong intense pulses at a higher peak current (8 A) resulted in the increased MRR (0.521 mm3/sec) and Ra (8.43 μm) leading to the formation of swages and ridges. The surface integrity analysis derived from Abbott–Firestone curve agreed that the lowest level has shown better skewness (Rsk = −0.274) and at highest level showed a larger deviation in skewness (Rsk = +2.672) signifies that higher asymmetry (poor) of the surface.
engineering, mechanical