Abstract:Voltage decay during cycling is still a major issue for Li-rich cathodes in lithium ion batteries. Recently, the increase of Ni content has been recognized as an effective way to mitigate this problem, although it leads to lower-capacity materials. To find a balance between voltage decay and high capacity, particles of Li-rich materials with concentration gradients of transition metals have been prepared. Since voltage decay is caused by oxygen loss and phase transition that occur mainly on the particle surface, the Ni content is designed with a negative gradient of concentration from the surface to the bulk of particles. To do so, microsized Li<sub>1.20</sub>Ni<sub>0.13</sub>Co<sub>0.13</sub>Mn<sub>0.54</sub>O<sub>2</sub> particles are mixed with much smaller LiNi<sub>0.8</sub>Co<sub>0.1</sub>Mn<sub>0.1</sub>O<sub>2</sub> particles to form deposits of small particles onto larger particles. The concentration gradient of Ni is achieved as the Ni ions in LiNi<sub>0.8</sub>Co<sub>0.1</sub>Mn<sub>0.1</sub>O<sub>2</sub> penetrate into Li<sub>1.20</sub>Ni<sub>0.13</sub>Co<sub>0.13</sub>Mn<sub>0.54</sub>O<sub>2</sub> during a calcination post-treatment. Gradient samples show superior cycling performance and voltage retention as well as improved safety. This systematic study explores a material model combining Li-rich and high-Ni layered cathodes that is shown to be effective in creating a balance between mitigated voltage decay and high energy density.The Supporting Information is available free of charge at <a class="ext-link" href="/doi/10.1021/acsami.0c10410?goto=supporting-info">https://pubs.acs.org/doi/10.1021/acsami.0c10410</a>.SEM and TEM images of the material before and after treatment, XRD patterns, XPS spectra, d<i>Q</i>/d<i>V</i> evolution during the cycling, rate performance, Nyquist plots of the prepared samples, and Raman spectrum of the pristine 10% NCM811 electrode (<a class="ext-link" href="/doi/suppl/10.1021/acsami.0c10410/suppl_file/am0c10410_si_001.pdf">PDF</a>)This article has not yet been cited by other publications.
materials science, multidisciplinary,nanoscience & nanotechnology
What problem does this paper attempt to address?