Hydrogen embrittlement susceptibility of AISI 4140 alloy-steel under cathodic protection and in H 2 S and CO 2 environment

Michel Motta Carvalho,Natália Feijó Lopes,Carlos Alexandre dos Santos,Roberto Moreira Schroeder,Eleani Maria da Costa
DOI: https://doi.org/10.1016/j.engfailanal.2024.108327
IF: 4
2024-04-18
Engineering Failure Analysis
Abstract:The susceptibility to hydrogen embrittlement (HE) of AISI 4140 steel when subjected to environments such as those found in offshore oil and gas fields is investigated. Hydrogen charging was carried out for 15 days using two different hydrogen sources, cathodic protection (CP) and corrosion in a saline solution containing high concentrations of H 2 S and CO 2 (SC-sour corrosion). The steel specimens were austenitized at 850 °C, oil-quenched at ambient temperature, followed by tempering for 18 min at 350, 450, and 600 °C. The effect of tempering temperatures on hydrogen embrittlement susceptibility was also investigated. Tensile strength testing, scanning electron microscopy (SEM), and fractography analysis were used to correlate the HE with microstructural and environmental conditions. The results revealed that both hydrogen charging conditions increased the steel hardness and decreased ductility, with this effect being more pronounced at lower tempering temperatures and SC-hydrogen charging. Fracture surfaces of the steel tempered at 600 °C with hydrogen charged exhibited predominantly ductile behavior with the presence of dimples, while at 350 and 450 °C surface fractures showed cleavage facets as a consequence of brittle behavior. In general, the AISI 4140 steel hydrogen embrittlement index (%EI) was higher for hydrogen charging induced by SC compared to CP.
engineering, mechanical,materials science, characterization & testing
What problem does this paper attempt to address?