Abstract:Inconel-718's compatibility with additive manufacturing (AM) has made it a center of attention for researchers. This paper focuses on how cooling rates affect the hardness of AM Inconel-718. To study the AM process, monocrystalline and polycrystalline Inconel-718 layers were added to a pristine substrate and equilibrated at 2000 K before being cooled to 300 K using cooling rates ranging from 5 K/ps to 100 K/ps, as well as an exponential cooling rate. The layers were then subjected to atomistic nanoindentation simulation to analyze the nanomechanical response, including hardness, dislocation density, microstructure, and surface imprints, at different cooling rates. Load-displacement (P-h) curves were plotted for each cooling rate. The findings of this study provide crucial insights into the effect of cooling rate on the nanoindentation-based response of additively manufactured Inconel-718. These insights can aid in the design of high-performance components for various applications
What problem does this paper attempt to address?
### Problems the Paper Attempts to Solve
This paper primarily investigates the effect of cooling rate on the nanoindentation performance of Inconel-718 prepared by additive manufacturing (AM). Specifically, the paper focuses on the following aspects:
1. **Effect of Cooling Rate on Hardness**: By using different cooling rates (from 5 K/ps to 100 K/ps, and exponential cooling rates), the study examines how the cooling process affects the hardness of Inconel-718.
2. **Microstructural Changes**: It explores how the microstructure of the material (including dislocation density, grain structure, and surface morphology) changes under different cooling rates.
3. **Nanoindentation Response**: Through atomic-scale nanoindentation simulations, the study analyzes the nanomechanical response under different cooling rates, including hardness, dislocation density, and surface imprint.
4. **Optimization of Mechanical Properties**: The aim is to provide key insights for designing high-performance AM components, especially for applications requiring high temperature, low thermal diffusivity, high corrosion resistance, and fatigue strength.
### Research Background
Inconel-718 is a Ni-Cr-Fe-based austenitic superalloy widely used in critical components in high-temperature environments, such as gas turbines, rockets, and aerospace, due to its high-temperature strength, low thermal diffusivity, high corrosion resistance, and fatigue strength. However, traditional processing methods face challenges when dealing with Inconel-718, such as high hardness, low thermal conductivity, and easy hardening. The emergence of additive manufacturing (AM) technology provides a new way to efficiently and precisely manufacture complex-shaped Inconel-718 components.
### Research Methods
1. **Atomic Structure Modeling**: Using LAMMPS software for large-scale atomic/molecular parallel simulations, single-crystal and polycrystalline Inconel-718 layers are constructed and deposited on a substrate.
2. **Additive Manufacturing Simulation**: The molten layer is heated to 2000 K and then cooled to 300 K at different cooling rates to simulate the actual AM process.
3. **Nanoindentation Simulation**: Through quasi-static nanoindentation simulations, the nanomechanical response under different cooling rates is analyzed, including load-displacement curves (P-h curves).
4. **Hardness Calculation**: The hardness of the material is calculated using the Oliver-Pharr method and the contact atom method.
### Main Findings
1. **Effect of Cooling Rate on Hardness**: Lower cooling rates (5 K/ps and 7.5 K/ps) result in lower material hardness, while higher cooling rates (10 K/ps and 15 K/ps) significantly increase material hardness. However, excessively high cooling rates (50 K/ps and 100 K/ps) lead to poor microstructure, reducing material hardness.
2. **Microstructural Changes**: Lower cooling rates favor the formation of more face-centered cubic (FCC) lattices, while higher cooling rates lead to more amorphous phases. Grain boundaries in polycrystalline structures can act as barriers to dislocations, reducing residual dislocations and slip planes, thereby increasing the proportion of FCC lattices.
3. **Nanoindentation Response**: P-h curves under different cooling rates show that higher cooling rates (10 K/ps and 15 K/ps) result in higher maximum loads, indicating that the material can withstand greater loads at the same indentation depth. However, excessively high cooling rates (50 K/ps and 100 K/ps) result in lower maximum loads, indicating poorer microstructure.
### Conclusion
This study, through atomic-scale simulations, thoroughly investigates the effect of cooling rate on the nanoindentation performance of additively manufactured Inconel-718, providing important theoretical basis for optimizing AM process parameters and designing high-performance components. These findings help to better understand the behavior of Inconel-718 at the nanoscale, thereby promoting its further development in various application fields.